50. 軸承鋼回火後的硬度會比淬火硬度低約
(A)HRC1~2
(B)HRC5~10
(C)HRC10~15
(D)HRC15~20。

答案:登入後查看
統計: A(17), B(2), C(2), D(0), E(0) #763073